POM-H


Brand:

  • Very good mechanical properties
  • Very good stiffness, hardness and creep resistance
  • Low coefficient of linear thermal expansion
  • Colours: white / black

Interested in this product?

Share

Semi-finished products made of virgin acetal homopolymer (POM-H).

It has better mechanical properties, stiffness, hardness and creep resistance, as well as a lower coefficient of thermal linear expansion than POM-C, and it often shows enhanced wear resistance.

It is physiologically inert and suitable for machining in automatic lathes; it is recommended for the manufacture of precision parts.

Properties ISO standard Unit of measurement Value
General properties      
Colour     natural / black
Density (specific weight) 1183 g/cm3 1.43
Water absorption 62 % 0.2
       
Mechanical properties      
Tensile strain at break 527 % 25
Tensile strain at yield 527 MPa 78
Tensile modulus of elasticity 527 MPa 3700
Impact strength 178/1eA kJ/m2 10
(Charpy impact test - notched)
Hardness 53505 Scale D 83
       
Thermal properties      
Melting temperature 11357 °C 180
Thermal conductivity 52612 W/mK 0.31
Coefficient of linear thermal expansion av. value between 20 °C and 60 °C m/mK 95x10-6
Working temperature, continuously -- °C -0.47619048
Working temperature, for short periods -- °C 150
Flammability UL94 -- HB/HB
       
Electric properties      
Dielectric strength 60243 kV/mm 20
Volume resistivity 60093 Ohm/cm >1014
Surface resistivity 60093 Ohm >1014
       
Physiological properties      
Suitable for contact with foodstuffs 21CFR (FDA) -- No